閱讀:358 發(fā)布時(shí)間:2018-6-19文獻(xiàn)名: Synthesis of MnO2/cellulose fiber nanocomposites for rapid adsorption of insecticide compound and optimization by response surface methodology
作者: Vinod Kumar Guptaa, AliFakhrib,d, Shilpi Agarwala, Nima Sadeghic
a Department of Applied Chemistry, University of Johannesburg, Johannesburg, South Africa
b Young Researchers and Elites Club, Science and Research Branch, Islamic Azad University, Tehran, Iran
d Department of Chemistry, Central Tehran Branch, Islamic Azad University, Tehran, Iran
c Department of Environmental Engineering, South Tehran Branch, Islamic Azad University, Tehran, Iran
摘要:The MnO2/Cellulose fiber Nanocomposites have been prepared via the microwave-assisted hydrothermal method. The characteristic structure of MnO2/Cellulose fiber Nanocomposites was analyzed using X-ray diffraction, photoluminescence and UV–vis spectra, Transmission electron Microscopy, N2 adsorption-desorption and Scanning electron microscopy instrumental techniques. BET surface area and crystallite size values of MnO2/cellulose fiber nanocomposites have been found as 87.064 m2/g and 70.0 nm, respectively. Response Surface Methodology (RSM) has been used for adsorption of Insecticide compound such as Toxaphene by prepared adsorbent. MnO2/Cellulose fiber Nanocomposites shows maximum removal of 96.5% at initial Toxaphene concentration of 5.0 mg/L, pH 3 and adsorbent dose of 5.0 g/L. Kinetic and equilibrium data follow pseudo-second order and Langmuir isotherm model, respectively. Adsorption capacity of MnO2/Cellulose fiber Nanocomposites has been found to be 5.465 mg/g.